ZHU Shi-zhen, LIU Yi-cheng, YU Xiao-dong. Continuous SiC Fiber Reinforced Glass Ceramic Matrix CompositesJ. Transactions of Beijing institute of Technology, 2000, (2): 257-260.
Citation: ZHU Shi-zhen, LIU Yi-cheng, YU Xiao-dong. Continuous SiC Fiber Reinforced Glass Ceramic Matrix CompositesJ. Transactions of Beijing institute of Technology, 2000, (2): 257-260.

Continuous SiC Fiber Reinforced Glass Ceramic Matrix Composites

  • To study the influence of the sinter temperature and the fiber volume fraction on the properties of the composites, BAS and MAS glasses were chosen as matrixes. The process of slurry impregnate and hot pressing was applied to the KD 1 SlC fiber reinforced glass ceramic matrix composites. The bending strength and the fracture toughness are 494. 1 MPa and 18. 28 MPa. m1/2 for SiCf/BAS, 538- 7 Mpa and 16. 70 MPa. m1/2 for SiCf/MAS. The failure mechanisms of the composites were studied.